Apparatus:  
 
Apparatus:  
*A large wide-mouthed jar - glass or clear plastic are both fine.
+
*A large wide-mouthed jar - glass or clear plastic are both fine,
 
*Tap water, and
 
*Tap water, and
 
*The aggregate to be tested.
 
*The aggregate to be tested.
    
Method:
 
Method:
# Collect approximately 5 cm of material in the jar (or at least two complete layers of 40 mm clear stone),  
+
# Collect approximately 5 cm of material in the jar (or at least two complete layers of 50 mm clear stone),  
 
# Add water to around 3/4 full,
 
# Add water to around 3/4 full,
 
# Secure cap and shake,  
 
# Secure cap and shake,  
 
# Leave for at least 30 minutes and until the water is clear - plan to run the test overnight when possible,
 
# Leave for at least 30 minutes and until the water is clear - plan to run the test overnight when possible,
# Examine the layer of sediment - if > 3 mm has been washed from 5 cm of product, reject the material,
+
# Examine the layer of sediment - if > 3 mm has been washed from 5 cm of product, the material should be rejected,
 
Note that the sediment may collect on top of, or at the bottom of the construction material.  
 